FIELD: metallurgy.
SUBSTANCE: method of red mud processing involves red mud pelletising, drying and further two-stage high temperature baking including oxidation baking stage at 1000-1150°C in air flow and reducing baking stage. Reducing baking stage is performed with feed of adiabatic catalytic conversion products from natural gas heated by gas flow from oxidation baking aggregate, to reducing reactor. Pelletised mud is dried by contact with natural gas heated to 260-450°C. Gas flow from oxidation baking aggregate is supplied both for natural gas heating and to production and superheating of water steam fed to a mix with natural gas.
EFFECT: enhanced hydrocarbon utilisation rate, reduced coke consumption and costs.
9 cl, 1 dwg, 2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MAKING PELLETS FOR METALLURGY | 2011 |
|
RU2487952C1 |
METAL COATING METHOD OF IRON-BEARING ORE-COAL RAW MATERIAL | 2011 |
|
RU2489493C2 |
METHOD FOR PRODUCING MAGNETITE PELLETS | 0 |
|
SU950784A1 |
0 |
|
SU539970A1 | |
METHOD OF PYROMETALLURGICAL ENRICHMENT OF COMPLEX IRON-CONTAINING MATERIALS | 1994 |
|
RU2087542C1 |
METALLIZED PRODUCT PRODUCTION METHOD | 0 |
|
SU985051A1 |
METHOD OF MAKING PELLETS FOR REDUCTION CASTING | 2010 |
|
RU2459879C2 |
METHOD OF METALLIZED PELLETS PRODUCTION | 2017 |
|
RU2688765C1 |
METHOD OF THE DIRECT REDUCTION OF THE FERRIC OXIDES AND PRODUCTION OF THE IRON MELT AND THE INSTALLATION FOR THE METHOD REALIZATION | 2005 |
|
RU2304620C2 |
METHOD OF COMPLEX REWORKING OF WASTES AFTER BURNING ORGANIC FUELS (VERSIONS) | 1998 |
|
RU2160318C2 |
Authors
Dates
2015-02-20—Published
2013-10-24—Filed