FIELD: metallurgy.
SUBSTANCE: oiled scale and red mud taken at 1:(0.6-1.0) ratio are added to water to get pulp to be subjected to aqueous leaching at S:L ratio of at least, 1.4 at 70-100°C and pulp mixing. Pulp is filtered to extract solid residue to be pelletised and roasted at 1050-1240°C, filtrate being subjected to cleaning.
EFFECT: roasted pellets for reduction casting.
3 cl, 7 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF REWORKING RED MUD OF ALUMINA PRODUCTION PROCESS | 2003 |
|
RU2245371C2 |
ANNEALING-FREE METHOD FOR PROCESSING FINE-GRAIN IRON -CONTAINING WASTE MATERIALS OF METALLURGICAL PRODUCTION INCLUDING OILED SCALE | 2000 |
|
RU2292405C2 |
METHOD OF PYROMETALLURGICAL ENRICHMENT OF COMPLEX IRON-CONTAINING MATERIALS | 1994 |
|
RU2087542C1 |
PROCEDURE FOR PRODUCTION OF AGGLOMERATE FOR MELTING IN BLAST FURNACE | 2009 |
|
RU2418079C2 |
METHOD OF RED MUD PROCESSING | 2013 |
|
RU2542177C1 |
METHOD OF PROCESSING OF PYRITE CINDERS | 2000 |
|
RU2172788C1 |
METHOD OF PROCESSING ZINC-CONTAINING WASTE OF FERROUS METALLURGY | 2005 |
|
RU2306348C1 |
PROCEDURE FOR RED MUD PROCESSING | 2009 |
|
RU2428490C2 |
RED MUD PROCESSING METHOD | 2019 |
|
RU2734423C1 |
METHOD FOR COMPLEX PROCESSING OF RED AND NEPHELINE SLUDGES | 2014 |
|
RU2619406C2 |
Authors
Dates
2012-08-27—Published
2010-10-04—Filed