FIELD: machine building.
SUBSTANCE: building-up welding of the hard alloy layer on back surfaces of axial cutting tools using the method of electrospark alloying is performed, which comprises the creation of carbide titanium or tungsten layer, or titanium boride or tungsten with cobalt or nickel binder with the width 80-90 mcm. The sharpening of back surfaces of the tool is performed with the rough tolerance for processing 20-30 mcm and the roughness Ra 0.8 mcm and additionally using the method of finishing plasma hardening a diamond-like silicon oxicarbonitrite-based coating with the width 1.5-2 mcm and with the hardness 53-54 GPa is applied.
EFFECT: increase of tool resistance and service life.
1 tbl, 12 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF RECONDITIONING PNEUMATIC SEEDER UNIT SEED DISC | 2012 |
|
RU2510318C2 |
METHOD OF HARDENING OF DISK FURROW OPENER CUTTING EDGE | 2020 |
|
RU2728198C1 |
METHOD OF RECONDITIONING PRECISION PARTS | 2009 |
|
RU2423214C1 |
STRENGTHENING COATING WITH REINFORCING EFFECT APPLICATION METHOD | 2005 |
|
RU2304185C1 |
GEAR CUTTER FOR CUTTING GEAR WHEELS | 1993 |
|
RU2068755C1 |
METHOD OF MANUFACTURE AND WORKING OF SHAPING TOOL, MAINLY, FOR FINISHING AMBER | 1998 |
|
RU2162780C2 |
ELECTRODE MATERIAL CHARGE FOR SPARK ALLOYING OF MACHINE PARTS | 2012 |
|
RU2515409C2 |
METHOD OF INCREASING WEAR-RESISTANCE OF WORKING SURFACES OF STEEL RING OF PULSE MECHANICAL SEALS | 2015 |
|
RU2631439C2 |
METHOD OF PREPARING ROLLS OF TUBE-ROLLING MILLS FOR OPERATION | 2008 |
|
RU2387503C1 |
DRILLING BIT, REINFORCED WITH DIAMOND CUTTING ELEMENTS | 2016 |
|
RU2625832C1 |
Authors
Dates
2015-04-10—Published
2013-12-26—Filed