FIELD: chemistry.
SUBSTANCE: invention relates to chemical industry and can be used in metal-finishing, for producing ceramic amour and in wear-resistant surfacing. A charge material consisting of a mixture of amorphous boron and fine carbon material is heated to 1700-1800°C for 15-20 minutes. The fine carbon material used is nano-fibre carbon.
EFFECT: invention reduces power consumption and prevents the appearance of free carbon impurities.
4 ex
Title | Year | Author | Number |
---|---|---|---|
ZIRCONIUM DIBORIDE PRODUCING METHOD | 2014 |
|
RU2559485C1 |
METHOD OF OBTAINING CHROME DIBORIDE | 2013 |
|
RU2549440C1 |
TITANIUM DIBORIDE PRODUCING METHOD | 2013 |
|
RU2559482C2 |
METHOD FOR OBTAINING A CHARGE FOR THE MANUFACTURE OF COMPOSITE CERAMICS BORON CARBIDE - CHROMIUM DIBORIDE | 2022 |
|
RU2789828C1 |
METHOD FOR PRODUCING A CHARGE FOR MANUFACTURING COMPOSITE BORON CARBIDE - ZIRCONIUM DIBORIDE CERAMICS | 2021 |
|
RU2770773C1 |
METHOD OF OBTAINING MIXTURES OF HIGH-DIFFERED HETEROGENEOUS POWDERS BASED ON BORON CARBIDE | 2018 |
|
RU2683107C1 |
METHOD OF PRODUCING VANADIUM CARBIDE | 2014 |
|
RU2599757C2 |
METHOD OF PRODUCING VANADIUM DIBORIDE | 2016 |
|
RU2638396C2 |
METHOD OF PRODUCTION OF ZIRCONIUM CARBIDE | 2014 |
|
RU2566420C1 |
METHOD OF PRODUCTION OF TITANIUM CARBIDE | 2013 |
|
RU2550182C2 |
Authors
Dates
2015-05-20—Published
2013-04-01—Filed