FIELD: metallurgy.
SUBSTANCE: method means rubbing through sieve of the charge having stoichiometric composition out of zirconium dioxide and carbon material with further heating in electric resistance furnace with graphite tube. At that heating is performed at temperature 1800-1900°C with holding at this temperature for 20-25 minutes, specific surface area of the carbon material is 138-160 m2/g, and nanofibre carbon is used as carbon material.
EFFECT: reduced power consumption during zirconium carbide production.
5 ex
Title | Year | Author | Number |
---|---|---|---|
ZIRCONIUM DIBORIDE PRODUCING METHOD | 2014 |
|
RU2559485C1 |
METHOD OF PRODUCING BORON CARBIDE | 2013 |
|
RU2550848C2 |
METHOD OF OBTAINING CHROME DIBORIDE | 2013 |
|
RU2549440C1 |
TITANIUM DIBORIDE PRODUCING METHOD | 2013 |
|
RU2559482C2 |
METHOD OF PRODUCING VANADIUM CARBIDE | 2014 |
|
RU2599757C2 |
METHOD OF PRODUCTION OF TITANIUM CARBIDE | 2013 |
|
RU2550182C2 |
METHOD OF PRODUCING VANADIUM DIBORIDE | 2016 |
|
RU2638396C2 |
METHOD FOR OBTAINING A CHARGE FOR THE MANUFACTURE OF COMPOSITE CERAMICS BORON CARBIDE - CHROMIUM DIBORIDE | 2022 |
|
RU2789828C1 |
METHOD FOR PRODUCING A CHARGE FOR MANUFACTURING COMPOSITE BORON CARBIDE - ZIRCONIUM DIBORIDE CERAMICS | 2021 |
|
RU2770773C1 |
METHOD FOR MANUFACTURING COMPOSITE CERAMICS BORON CARBIDE - ZIRCONIUM DIBORIDE | 2023 |
|
RU2812539C1 |
Authors
Dates
2015-10-27—Published
2014-04-29—Filed