FIELD: chemistry.
SUBSTANCE: invention relates to obtaining fireproof polyurethane foam from foamed reaction mixture, which consists of mixture of polyols, polyisocyanate and fireproof additives (fire-retardants). Composition for obtaining fireproof polyurethane foam is described, which contains mixture of polyols, polyisocyanate and fireproof additives, with mixture of ammonium polyphosphate and ammonium sulphamate being applied as additives in quantity from 10 to 40 wt % of the total amount of components, and ratio of ammonium polyphosphate to ammonium sulphamate in mixture constitutes respectively from 1:2 to 7:1 weight parts.
EFFECT: obtaining polyurethane foam, which has maximal fire resistance (flammability group G-1), practically invariable density in comparison with polyurethane foam, obtained without fireproof additives.
2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING FOAM POLYISOCYANURATE OF HIGH FIRE RESISTANCE | 2020 |
|
RU2733510C1 |
METHOD FOR PRODUCING FIRE-RESISTANT RIGID POLYURETHANE FOAM | 2022 |
|
RU2805414C1 |
SOUND-ABSORBING MATERIAL FOR TRUCK SOUND-ABSORBING SCREENS WITH REDUCED FLAMMABILITY | 2022 |
|
RU2800220C1 |
COMPOSITION FOR FIRE-RESISTANT FOAMED POLYURETHANE | 2019 |
|
RU2714917C1 |
METHOD OF PRODUCTION OF FIREPROOF POLYURETHANE FOAM | 2004 |
|
RU2268899C1 |
COMPOSITION FOR PRODUCTION OF RIGID FOAMED POLYURETHANE WITH LOW FLAMMABILITY | 2019 |
|
RU2726212C1 |
METHOD OF PRODUCING FILLED POLYURETHANE FOAM FOR HEAT-INSULATING PRODUCTS | 1998 |
|
RU2123013C1 |
FIRE-RESISTANT POLYURETHANE FOAM PRODUCTION PROCESS | 2006 |
|
RU2296777C1 |
POLYESTER BINDER OF REDUCED FLAMMABILITY | 2017 |
|
RU2674210C1 |
METHOD OF PRODUCING FIRE-RESISTANT POLYURETHANE FOAM WITH GOOD LASTING OPERATIONAL PROPERTIES | 2010 |
|
RU2540950C2 |
Authors
Dates
2015-07-10—Published
2014-07-07—Filed