FIELD: electricity.
SUBSTANCE: composition, wt % is obtained of high-pressure polyethylene - 59.6-79.6, filling material with polar surface - microcalcite - 20.0-40.0, calcium stearate - 0.3 and Richnox 1010 - 0.1. The filling material is pre-dried at 105°C up to absolutely dry state.
EFFECT: invention allows increase in homogeneity of produced composition due to hydrophobisation of the filling material surface.
2 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING ELECTRICAL INSULATING COMPOUND | 2016 |
|
RU2617165C1 |
METHOD OF MANUFACTURING SELF-EXTINGUISHING CABLES EMITTING LOW LEVELS OF SMOKE AND FLAMEPROOF COMPOSITIONS UTILIZED THEREIN | 1999 |
|
RU2237078C2 |
FLEXIBLE FIREPROOF SELF-EXTINGUISHING ELECTRIC CABLE | 2013 |
|
RU2548565C2 |
POLYMER COMPOSITION FOR AN ANTICORROSIVE COATING | 2021 |
|
RU2775000C1 |
FIRE-RESISTANT SELF-QUENCHING CABLE OR WIRE | 2004 |
|
RU2285306C2 |
METHOD OF PREPARING CELLULOSE-CONTAINING POLYMER SUPER-CONCENTRATE AND COMPOSITE MATERIALS BASED ON SAID SUPER-CONCENTRATE | 2009 |
|
RU2424263C1 |
POLYMER COMPOSITION FOR ANTI-CORROSION COATING | 2018 |
|
RU2683079C1 |
REPAIR ADHESIVE COMPOSITION | 2009 |
|
RU2412973C1 |
METHOD OF PRODUCING POLYMER DIELECTRIC | 2023 |
|
RU2821113C1 |
RAW MIX FOR PRODUCTION OF MODIFIED GYPSUM COMPOSITE MATERIALS | 2013 |
|
RU2539478C1 |
Authors
Dates
2016-01-20—Published
2014-05-30—Filed