FIELD: process engineering.
SUBSTANCE: article and current conducting material are arranged in the processing zone to be rarefied. Negative potential is fed to the article and to the current conducting material. Note here that said current conducting material consists of at least two components each being a metal or an alloy. Vacuum arc is excited alternatively at each component of current conducting material. Current conducting material ions are accumulated and diffused on the article surface in the medium of shielding gas or in the medium of reactive gas and inert argon gas at the negative potential at the article of 60-180 V and intermittent bombardment of the article surface by gas ions of 20-40 keV energy.
EFFECT: higher erosion and stable heat resistance.
4 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR APPLICATION OF COATING | 2009 |
|
RU2415199C1 |
METHOD OF PRODUCTION OF WEAR-RESISTANT HIGH-TEMPERATURE COATING | 2014 |
|
RU2570274C1 |
METHOD OF PRODUCING ANTI-FRETTING COATING | 2015 |
|
RU2603414C1 |
METHOD FOR PRODUCING EROSION-CORROSION-RESISTANT COATING ON SURFACE OF TITANIUM ALLOY PRODUCT | 2023 |
|
RU2808481C1 |
METHOD FOR FABRICATED METALLIC PRODUCT SURFACE TREATMENT | 2007 |
|
RU2340704C2 |
METHOD OF WORKING SURFACE OF METALLIC ARTICLE | 2006 |
|
RU2308537C1 |
METHOD FOR OBTAINING AN ANTI-FRETTING COATING | 2022 |
|
RU2777090C1 |
METHOD OF MACHINING METAL PART | 2007 |
|
RU2368701C2 |
METHOD OF PROCESSING SURFACE OF ARTICLE MADE FROM TITANIUM ALLOY | 2010 |
|
RU2445406C1 |
METHOD OF PRODUCING DAMPING COATING | 2015 |
|
RU2598425C1 |
Authors
Dates
2016-02-10—Published
2015-03-20—Filed