FIELD: chemistry.
SUBSTANCE: glaze includes, wt %: quartz sand 45.5-54.5; red lead 20-25; potash 10-15; soda 1-2; cobalt oxide 0.5-1; copper oxide 0.5-1; portland cement 5-7; drill 5-7.
EFFECT: increased frost resistance.
1 tbl