FIELD: chemistry.
SUBSTANCE: method comprises sequential administration of bitumen under agitation at 150-160°C plasticiser, which is used as tall oil, a polymer in the form of a block copolymer of butadiene and styrene, styrene-butadiene-styrene, stearic acid, epoxy resin and mixing of all the components for 1.5 hours at a temperature of 150-160°C to complete dissolution, then the resulting mixture is introduced polyethylenepolyamine and stirred for 10-15 min at a temperature of 150-160°C.
EFFECT: improving homogeneity of polymer-bitumen, its physical-mechanical characteristics, reduction of time and the cooking temperature of polymer-asphalt astringent and development stage process it is received.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMER-BITUMEN BINDER AND METHOD FOR PRODUCTION THEREOF | 2012 |
|
RU2496812C1 |
POLYMER-BITUMEN BINDER AND METHOD FOR ITS PREPARATION | 2020 |
|
RU2754709C2 |
COMPOSITION AND METHOD FOR OBTAINING MODIFIED BITUMEN FOR ROAD CONSTRUCTION | 2022 |
|
RU2798340C1 |
POLYMER-ASPHALT BINDER FOR ROAD SURFACE AND METHOD FOR PRODUCTION THEREOF | 2011 |
|
RU2477736C2 |
POLYMER-BITUMEN BINDER WITH INCREASED RESISTANCE TO SHEAR DEFORMATIONS AND METHOD FOR PRODUCTION THEREOF | 2020 |
|
RU2765646C1 |
BITUMEN COMPOSITION | 2001 |
|
RU2226203C2 |
POLYMERIC-BITUMEN BINDING AGENT AND METHOD FOR ITS PREPARING | 2003 |
|
RU2241724C1 |
POLYMER-BITUMEN BINDER FOR ROAD SURFACE AND METHOD FOR PRODUCTION THEREOF | 2016 |
|
RU2639902C1 |
METHOD OF PRODUCING COMPOSITE BITUMEN BINDER FOR ROAD CONSTRUCTION | 2023 |
|
RU2816688C1 |
A METHOD FOR PRODUCING A BITUMEN BINDER WITH IMPROVED VISCOELASTIC AND ADHESIVE CHARACTERISTICS | 2022 |
|
RU2785849C1 |
Authors
Dates
2017-05-11—Published
2015-12-23—Filed