FIELD: chemistry.
SUBSTANCE: method for producing impregnated sorbent is proposed, comprising preparing the impregnation solution, the impregnating additive, the base impregnating, maturing and heat treatment. The base is represented by ion-exchange resin with a total pore volume of 0.80-0.87 cm3/g. The impregnating additive is represented by finely divided activated carbon with the size of micropores having the half width of 0.56-0.60 nm. The heat treatment is carried out at the temperature of 70-78°C.
EFFECT: invention allows to obtain impregnated sorbent for extracting the rare earth element lanthanum from aqueous solution, having the increased sorptive activity as per lanthanum.
3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING IMPREGNATED SORBENT | 2011 |
|
RU2461420C1 |
METHOD OF PRODUCTION OF SORBENT-CATALYST | 2005 |
|
RU2281158C1 |
METHOD FOR PRODUCING HERBICIDE STABILISED WITH ACTIVE CARBON | 2020 |
|
RU2752319C1 |
METHOD FOR OBTAINING POWDER SORBENT | 2014 |
|
RU2572144C1 |
METHOD OF OBTAINING IMPREGNATED ELASTIC SORBENT | 2014 |
|
RU2568485C1 |
METHOD OF OBTAINING ACTIVE COAL | 2011 |
|
RU2471708C1 |
METHOD OF PRODUCTION OF ADSORBENT | 2003 |
|
RU2228792C1 |
METHOD OF OBTAINING CHEMOSORBENT | 2012 |
|
RU2510868C1 |
AMMONIA AND HYDROGEN SULFIDE ABSORBENT AND A METHOD FOR PREPARATION THEREOF | 2002 |
|
RU2210429C1 |
METHOD OF PREPARING IMPREGNATED ADSORBENT | 1998 |
|
RU2133217C1 |
Authors
Dates
2017-06-13—Published
2016-07-08—Filed