FIELD: construction.
SUBSTANCE: raw mix for producing silicate bricks, including lime and water, additionally contains sulfite-cellulose bard - SCB and burnt earth - waste foundry, incurred to co-grinding with lime to a specific surface of 2500-3000 g/cm2, with the following ratio of components, wt %: burnt earth 92-94, lime 6-8, SCB 0.1-0.3 from the mass of lime over 100, water - up to 5-7% moisture of the press powder.
EFFECT: increasing the strength of silicate brick, reducing the cost of its production, expanding the raw base, recycling the waste of the foundry.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
RAW MIX FOR MAKING SILICA BRICK | 0 |
|
SU1016266A1 |
METHOD OF MANUFACTURING SILICATE BRICK AND RAW MIX FOR THEREOF | 1999 |
|
RU2162454C1 |
RAW MIXTURE | 2007 |
|
RU2380332C2 |
METHOD FOR PRODUCTION OF BUILDING MATERIALS FROM HIGH-BASICITY METALLURGICAL SLAGS | 0 |
|
SU1776253A3 |
SILICATE BRICK FABRICATION PROCESS | 2001 |
|
RU2213071C2 |
RAW MATERIALS MIX FOR PRODUCING SILICATE EXTRUDED PRODUCTS | 2015 |
|
RU2614830C2 |
RAW MIXTURE FOR PRODUCTION OF BUILDING CERAMIC PRODUCTS | 2020 |
|
RU2748199C1 |
METHOD FOR PRODUCTION OF RAW MATERIALS MIXTURE FOR MANUFACTURING OF SILICATE BRICK | 1995 |
|
RU2096375C1 |
MIXTURE FOR PRODUCTION OF SILICATE BRICK | 2018 |
|
RU2703061C1 |
METHOD FOR MANUFACTURING RAW MIXTURE FOR CALCIUM SILICATE BRICK FABRICATION | 1995 |
|
RU2331604C2 |
Authors
Dates
2017-08-02—Published
2015-10-08—Filed