FIELD: metallurgy.
SUBSTANCE: intermetallide Pd5Ba is produced by melting, is ground in an atmosphere of inert gas or CO2 to obtain a powder, the resulting powder is mixed with palladium powder and mechanically activated by the planetary or vibrator mill for 5-15 minutes. The powder obtained after mechanoactivation is compressed, and the compact is sintered in an argon atmosphere in a beam of fast electrons at a temperature of (700-800)°C for 25-40 minutes.
EFFECT: increasing the coefficient of secondary electron emission of the pressed metal-alloy cathodes Pd-Ba.
2 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING CATHODE MATERIAL BASED ON METAL OF PLATINUM GROUP AND BARIUM | 2016 |
|
RU2646654C2 |
METHOD FOR PRODUCING CATHODE ALLOY BASED ON METAL OF PLATINUM GROUP AND BARIUM | 2016 |
|
RU2627709C1 |
PRESSED METAL-ALLOY PALLADIUM-BARIUM CATHODE AND METHOD OF ITS OBTAINING | 2016 |
|
RU2647388C2 |
METHOD OF PRODUCING FINE POWDER OF INTERMETALLIDE PDBA | 2019 |
|
RU2741940C1 |
MAGNETRON WITH NON-FILAMENT CATHODE | 2008 |
|
RU2380784C1 |
METHOD OF PRODUCING EMISSION-ACTIVE CATHODE ALLOY | 2014 |
|
RU2581151C1 |
PROCESS OF MANUFACTURE OF SECONDARY EMISSION CATHODE | 1990 |
|
RU2069915C1 |
METHOD FOR OBTAINING FERRITE PRODUCTS | 2016 |
|
RU2664745C2 |
METHOD FOR OBTAINING POLYCRYSTALLINE GARNET-TYPE FERRITES | 2017 |
|
RU2660493C1 |
PULSE MAGNETRON WITH NON-INCANDESCENT START WITH A THREE-MODULE ACTIVE BODY IN THE CATHODE UNIT | 2021 |
|
RU2776305C1 |
Authors
Dates
2017-08-10—Published
2016-08-02—Filed