FIELD: packaging industry.
SUBSTANCE: housing formed of a glass composition of Type I, Class B, in accordance with standard ASTM E438-92, the housing having HGB2 hydrolytic resistance class or higher according to ISO 719. Casing glass container is strengthened by ion exchange. On the outer surface of the housing is located a smooth coating the organic layer. The outer surface of the housing with a smooth coating layer has a friction coefficient of less than or equal to 0.7. The coating layer is thermally stable at a temperature of at least about 260°C for 30 minutes.
EFFECT: increased resistance to delamination, damage, increase the strength of the glass container.
10 cl, 51 dwg, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
GLASS CONTAINERS WITH RESISTANCE TO DELAMINATION AND HIGH RESISTANCE TO DAMAGE | 2013 |
|
RU2706146C2 |
GLASS CONTAINERS WITH IMPROVED STRENGTH AND DELAMINATION RESISTANCE | 2013 |
|
RU2658852C2 |
GLASS CONTAINERS WITH DELAMINATION RESISTANCE AND IMPROVED DAMAGE TOLERANCE | 2013 |
|
RU2659928C2 |
STRENGTHENED GLASS CONTAINERS, RESISTANT TO DELAMINATION AND DAMAGE | 2013 |
|
RU2657265C2 |
GLASS CONTAINERS WITH IMPROVED STRENGTH AND IMPROVED RESISTANCE TO DESTRUCTION | 2013 |
|
RU2706846C2 |
GLASS CONTAINERS WITH IMPROVED STRENGTH AND IMPROVED DAMAGE TOLERANCE | 2013 |
|
RU2679454C2 |
METHOD FOR MANUFACTURING PHARMACEUTICAL CONTAINER | 2019 |
|
RU2733518C1 |
COATED PHARMACEUTICAL PACKAGE (VERSIONS) | 2018 |
|
RU2708594C1 |
GLASS PRODUCTS WITH ANTI-FRICTION COATINGS | 2013 |
|
RU2641817C2 |
COATED PHARMACEUTICAL PACKAGING (OPTIONS) | 2013 |
|
RU2671328C2 |
Authors
Dates
2017-10-24—Published
2013-10-23—Filed