FIELD: layered products.
SUBSTANCE: invention relates to glass containers. Glass container includes a body having an inner surface, an outer surface and a wall thickness that is between the outer surface and the inner surface. Inner surface of the body has a delamination factor of less than or equal to 10. Body has a compression-stressed layer extending from the outer surface of the housing into the wall thickness. Compression-stressed layer can have a surface compressive stress of more than or equal to 150 MPa. Lubricous coating positioned around is at least a portion of the outer surface of the body. Outer surface of the body with the lubricous coating has a friction coefficient of less than or equal to 0.7.
EFFECT: technical result is an increase in strength, resistance to delamination and damage.
44 cl, 58 dwg, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
GLASS CONTAINERS WITH IMPROVED STRENGTH AND DELAMINATION RESISTANCE | 2013 |
|
RU2658852C2 |
GLASS CONTAINERS WITH DELAMINATION RESISTANCE AND IMPROVED DAMAGE TOLERANCE | 2013 |
|
RU2659928C2 |
GLASS CONTAINERS WITH RESISTANCE TO DELAMINATION AND HIGH RESISTANCE TO DAMAGE | 2013 |
|
RU2706146C2 |
DELAMINATION RESISTANT GLASS CONTAINERS | 2013 |
|
RU2674269C2 |
GLASS CONTAINERS WITH IMPROVED STRENGTH AND IMPROVED DAMAGE TOLERANCE | 2013 |
|
RU2679454C2 |
CONTAINERS OF A STRENGTHENED BOROSILICATE GLASS WITH INCREASED DAMAGE TOLERANCE | 2013 |
|
RU2634133C2 |
GLASS CONTAINERS WITH IMPROVED STRENGTH AND IMPROVED RESISTANCE TO DESTRUCTION | 2013 |
|
RU2706846C2 |
METHODS OF PROCESSING GLASS ARTICLES | 2015 |
|
RU2711424C2 |
GLASS PRODUCTS WITH ANTI-FRICTION COATINGS | 2013 |
|
RU2641817C2 |
RESISTANT TO STRATIFICATION CONTAINERS WITH HEAT-RESISTANT COATINGS | 2013 |
|
RU2634758C2 |
Authors
Dates
2018-06-09—Published
2013-11-22—Filed