FIELD: glass; mineral and slag wool.
SUBSTANCE: invention relates to glass containers. Glass container includes a body having an inner surface, an outer surface and a wall thickness that is between the outer surface and the inner surface. Inner surface of the body has a delamination factor of less than or equal to 10. Coating layer having a friction coefficient of 0.07 or less is applied to the outer surface of the body. Coating layer can be inorganic or organic, or temporary.
EFFECT: technical result is an increase in strength, resistance to delamination and damage.
38 cl, 57 dwg, 3 tbl, 23 ex
Title | Year | Author | Number |
---|---|---|---|
GLASS CONTAINERS WITH RESISTANCE TO DELAMINATION AND HIGH RESISTANCE TO DAMAGE | 2013 |
|
RU2706146C2 |
GLASS CONTAINERS WITH IMPROVED STRENGTH AND DELAMINATION RESISTANCE | 2013 |
|
RU2658852C2 |
CONTAINERS OF A STRENGTHENED BOROSILICATE GLASS WITH INCREASED DAMAGE TOLERANCE | 2013 |
|
RU2634133C2 |
STRENGTHENED GLASS CONTAINERS, RESISTANT TO DELAMINATION AND DAMAGE | 2013 |
|
RU2657265C2 |
GLASS CONTAINERS WITH IMPROVED STRENGTH AND IMPROVED DAMAGE TOLERANCE | 2013 |
|
RU2679454C2 |
GLASS CONTAINERS WITH IMPROVED STRENGTH AND IMPROVED RESISTANCE TO DESTRUCTION | 2013 |
|
RU2706846C2 |
DELAMINATION RESISTANT GLASS CONTAINERS | 2013 |
|
RU2674269C2 |
GLASS PRODUCTS WITH ANTI-FRICTION COATINGS | 2013 |
|
RU2641817C2 |
RESISTANT TO STRATIFICATION CONTAINERS WITH HEAT-RESISTANT COATINGS | 2013 |
|
RU2634758C2 |
METHOD FOR MANUFACTURING PHARMACEUTICAL CONTAINER | 2019 |
|
RU2733518C1 |
Authors
Dates
2018-07-04—Published
2013-11-22—Filed