FIELD: technological processes.
SUBSTANCE: invention can be used for making butt joints of details made of aluminium heat-resistant alloys of thickness 2…6 mm. A welding tool with a pin is used made in the form of a flattened cone with a length of 1.8…5.7 mm with three "left" thread grooves, and a supporting ledge with a diameter of 8…18 mm with a spiral groove. The tool is immersed into the joint of the connected details with a minimum speed of the vertical displacement 7…12 mm/min and high rotation velocity 350…500 rpm until a predetermined depth of 90…95% of the thickness of the welded details is achieved. The angle of the tool is changed relative to the vertical axis from 0 to -1.5…-2.5°. Then, keeping the angle and rotation velocity, the tool is moved along the joint line at a speed of 220…300 mm/min at a constant axial force of 12…15 kN, controlled by feedback sensors.
EFFECT: tool runout is prevented, internal defects are eliminated and the strength of the welded joint is ensured.
2 dwg
Title | Year | Author | Number |
---|---|---|---|
FRICTION WELDING METHOD WITH ALUMINIUM WROUGHT ALLOYS MIXING | 2016 |
|
RU2634402C1 |
METHOD OF FRICTION WELDING WITH MIXING OF JOINTS OF ALUMINIUM ALLOYS | 2018 |
|
RU2686494C1 |
METHOD OF FRICTION WELDING WITH MIXING OF ALUMINIUM ALLOY BUTT JOINTS | 2007 |
|
RU2412034C2 |
HIGH-STRENGTH ALUMINUM-LITHIUM ALLOYS OF THE Al-Cu-Li SYSTEM BUTT JOINTS FRICTION WITH MIXING WELDING METHOD | 2017 |
|
RU2679787C1 |
METHOD FOR FRICTION WELDING OF ALUMINIUM ALLOYS | 2006 |
|
RU2350443C2 |
METHOD OF COMBINED FRICTION WELDING OF TEE JOINTS | 2011 |
|
RU2466839C1 |
METHOD FOR FRICTION WELDING OF ALUMINUM ALLOY BUTT JOINTS | 2003 |
|
RU2247639C1 |
TOOL FOR FRICTION STIR WELDING | 2015 |
|
RU2621514C2 |
METHOD OF FRICTION WELDING BY ROTARY DISC | 2012 |
|
RU2496621C1 |
TOOL FOR FRICTION WELDING WITH MIXING OF ALUMINIUM ALLOYS AND METHOD OF WELDING | 2007 |
|
RU2357843C2 |
Authors
Dates
2017-10-26—Published
2016-06-20—Filed