FIELD: electricity.
SUBSTANCE: method comprises depositing a coating of an electrolyte containing iron chloride 350-400 kg/m3, cobalt chloride 5-50 kg/m3, hydrochloric acid 0.5-2.0 kg/m3 and water on an alternating asymmetric current with current asymmetry coefficient of 1.2-6.0 at an electrolyte temperature of 30-50°C. Sodium chloride in an amount of 5-20 kg/m3 is administered into the electrolyte composition, and the deposition is carried out in the interval of cathode current densities of 60-100 A/dm2.
EFFECT: increasing the stability of the electrolyte, preventing its rapid oxidation, increasing the electrical conductivity of the electrolyte and the rate of the coating deposition.
1 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-ALUMINUM ALLOY | 2003 |
|
RU2263727C2 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-BORON ALLOY | 2019 |
|
RU2705843C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF AN IRON-TITANIUM ALLOY | 2003 |
|
RU2230139C1 |
METHOD OF ELECTROLYTIC PRECIPITATION OF IRON-MOLYBDENUM DISULFIDE COATING | 2013 |
|
RU2537686C1 |
METHOD OF ELECTROLYTIC DEPOSTION OF IRON-VANADIUM-COBALT ALLOY | 2009 |
|
RU2401328C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-BORON ALLOY-BASED COAT | 2003 |
|
RU2250936C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-ALUMINIUM ALLOY | 2012 |
|
RU2486294C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-COBALT ALLOY | 2002 |
|
RU2230836C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-VANADIUM ALLOY | 2002 |
|
RU2231578C1 |
METHOD OF ELECTRODEPOSITION OF IRON-PHOSPHORUS ALLOY | 1999 |
|
RU2164560C1 |
Authors
Dates
2017-10-31—Published
2015-12-21—Filed