FIELD: metallurgy.
SUBSTANCE: deposition is carried out at AC asymmetric current with asymmetry coefficient of 1.2…6 and current frequency of 50 Hz from electrolyte containing the following components in wt %: iron chloride 300…400, sodium vanadate 5…8, citric acid 7…12, cobalt chloride 10…15, sulphuric acid 1.5…2.0 at electrolyte temperature of 20…40°C and interval of cathode current densities of 15…40 A/dm2.
EFFECT: micro hardness of deposited coat makes 9200 MPa, friction coefficient makes 0,03.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-VANADIUM ALLOY | 2002 |
|
RU2231578C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-TUNGSTEN ALLOY | 2001 |
|
RU2192509C2 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-COBALT ALLOY | 2002 |
|
RU2230836C1 |
METHOD OF ELECTRODEPOSITION OF FERROMOLYBDENUM ALLOY | 2000 |
|
RU2174163C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-TITANIUM-COBALT ALLOY | 2009 |
|
RU2410473C1 |
METHOD OF ELECTRODEPOSITION OF IRON-PHOSPHORUS ALLOY | 1999 |
|
RU2164560C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-ALUMINUM ALLOY | 2003 |
|
RU2263727C2 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-BORON ALLOY-BASED COAT | 2003 |
|
RU2250936C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF AN IRON-TITANIUM ALLOY | 2003 |
|
RU2230139C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-COBALT ALLOY | 2015 |
|
RU2634555C2 |
Authors
Dates
2010-10-10—Published
2009-05-19—Filed