FIELD: electrolytic deposition of wear-resisting coatings for recovery and reinforcement of the worn surfaces of details. SUBSTANCE: the invention presents a method of electrolytic deposition of an iron-titanium alloy and is dealt in particular with electrolytic deposition of wear-resisting coatings for recovery and reinforcement of the worn surfaces of details. The method provides for deposition of coatings from the electrolyte, that contains (in kg / m3): iron chloride - 350-400, titanium oxalate - 15-25, saline acid - 0.5-1.5. The deposition is exercised using an alternating asymmetric current with an asymmetry factor of 1.2-6.0 at the electrolyte temperature of 20-40o, an interval of cathode current densities of 35-50 A/dcm2. Technical result: increased efficiency of the method, strengthened linkage of the coating with the base, increased microhardness and wear resistance. EFFECT: the invention allows to increase strength of linkage of the coating with the base, microhardness and wear resistance of products, general efficiency of the method.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-BORON ALLOY-BASED COAT | 2003 |
|
RU2250936C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-ALUMINUM ALLOY | 2003 |
|
RU2263727C2 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-VANADIUM ALLOY | 2002 |
|
RU2231578C1 |
METHOD OF ELECTROLYTIC PRECIPITATION OF IRON-MOLYBDENUM DISULFIDE COATING | 2013 |
|
RU2537686C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-ALUMINIUM ALLOY | 2012 |
|
RU2486294C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-COBALT ALLOY | 2002 |
|
RU2230836C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF COMPOSITE COATING IRON - TITANIUM - MOLYBDENUM DISULPHIDE | 2024 |
|
RU2818197C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-TUNGSTEN ALLOY | 2001 |
|
RU2192509C2 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-COBALT ALLOY | 2015 |
|
RU2634555C2 |
METHOD OF ELECTRODEPOSITION OF IRON-PHOSPHORUS ALLOY | 1999 |
|
RU2164560C1 |
Authors
Dates
2004-06-10—Published
2003-03-05—Filed