FIELD: electrodeposition of solid wear-resistant coatings, particularly, iron-phosphorus coatings for reconditioning and hardening of part surfaces. SUBSTANCE: deposition is carried out from electrolyte containing, g/l: ferrous chloride, 350-400; hydrochloric acid, 0.6-0.8; sodium hypophosphite, 2-12. Use is made of alternating asymmetric current with asymmetry coefficient of 1.2-6, cathode current density of 35-45 A/sq.dm, and electrolyte temperature of 30-50 C. EFFECT: higher efficiency due to produced coatings with high microhardness and wear resistance. 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ELECTRODEPOSITION OF FERROMOLYBDENUM ALLOY | 2000 |
|
RU2174163C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-COBALT ALLOY | 2002 |
|
RU2230836C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-VANADIUM ALLOY | 2002 |
|
RU2231578C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF AN IRON-TITANIUM ALLOY | 2003 |
|
RU2230139C1 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-ALUMINUM ALLOY | 2003 |
|
RU2263727C2 |
METHOD FOR ELECTROLYTIC DEPOSITION OF IRON-BORON ALLOY-BASED COAT | 2003 |
|
RU2250936C1 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-TUNGSTEN ALLOY | 2001 |
|
RU2192509C2 |
METHOD OF ELECTROLYTIC DEPOSITION OF IRON-CHROMIUM ALLOY | 2005 |
|
RU2285065C1 |
ELECTROLYTE FOR DEPOSITION OF COAT | 1999 |
|
RU2169799C1 |
ELECTROLYTE FOR COAT DEPOSITION | 2003 |
|
RU2250935C1 |
Authors
Dates
2001-03-27—Published
1999-11-02—Filed