FIELD: metallurgy.
SUBSTANCE: model unit of the thermite charge is made by size 5-10% less than required size of the casting and placed in press-mould, which cavity corresponds to the required dimensions and configuration of the casting. A wax-like pattern material powder is metered into the mould which is pressed onto the model block under a pressure of 0.5-2.5 mpa. A shell-type solid mould is obtained by applying layers of refractory slurry to the model block. The shell-type mould is moulded into a refractory filler, calcinated, and the model block is ignited for exothermal reaction with formation of steel melt in the shell-type mould.
EFFECT: increase of dimensional and geometric accuracy of the castings.
3 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF RECEIVING OF STEEL CASTINGS | 2006 |
|
RU2367539C2 |
METHOD OF RECEIVING OF STEEL CASTINGS | 2006 |
|
RU2367540C2 |
BIMETALLIC CASTING METHOD | 2018 |
|
RU2697995C1 |
BIMETALLIC CASTING METHOD | 2018 |
|
RU2696118C1 |
CASTING MOULD WITH THERMITE RISER | 2008 |
|
RU2372164C1 |
EXOTHERMIC MIXTURE FOR HEATING OF MOLD HOT TOP | 1996 |
|
RU2108889C1 |
DEVICE FOR PRODUCING IRON-CARBON-ALLOY CASTINGS | 2017 |
|
RU2658682C1 |
METHOD OF MAKING CASTINGS OF FERROUS AND NON-FERROUS METALS | 1992 |
|
RU2048955C1 |
EXOTHERMAL MIXTURE FOR HEATING RISER PORTIONS OF CASTING MOULDS | 0 |
|
SU598684A1 |
METHOD FOR MANUFACTURE OF MOLD RISER | 1992 |
|
RU2015835C1 |
Authors
Dates
2017-11-03—Published
2016-05-13—Filed