FIELD: chemistry.
SUBSTANCE: product contains a propylene copolymer (R-PP) having a melt flow rate MFR2 (230°C) of 0.5 to 4.0 g/10 minutes, and a fraction soluble in hexane of 1.8 to 5.0 wt %. The propylene copolymer (R-PP) has a comonomer content in the range of 3.0 to 10.0 mol %, wherein the comonomer is ethylene. In addition, the propylene copolymer (R-PP) has a relative content of individual ethylene sequences (I(E)) with respect to the block ethylene sequences of 45.0 to 69.0%.
EFFECT: high BAF performance, high impact resistance, improved optical properties.
16 cl, 3 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| BLOW MOLDED PRODUCT WITH GOOD MECHANICAL AND OPTICAL PROPERTIES | 2014 |
|
RU2648674C2 |
| SOFT AND TRANSPARENT COPOLYMERS OF PROPYLENE | 2017 |
|
RU2698721C1 |
| PROPYLENE COPOLYMER FOR THIN-WALL PACKAGING | 2014 |
|
RU2652110C2 |
| POLYPROPYLENE FOR FILM APPLICATION | 2014 |
|
RU2648675C2 |
| PROPYLENE STATISTICAL COPOLYMER FOR APPLICATION IN FILMS | 2015 |
|
RU2668797C2 |
| MULTI-MODAL POLYPROPYLENE WITH REGARD TO THE CO-MONOMER CONTENT | 2014 |
|
RU2657872C1 |
| PROCESS FOR PRODUCTION OF POLYPROPYLENE WITH HIGH POLYDISPERSITY | 2014 |
|
RU2648672C2 |
| CABLE SHEATH | 2018 |
|
RU2746595C1 |
| CABLE SHEATH | 2018 |
|
RU2761387C1 |
| POLYPROPYLENE WITH EXTREMELY WIDE MOLECULAR WEIGHT DISTRIBUTION | 2014 |
|
RU2673339C2 |
Authors
Dates
2017-12-08—Published
2014-06-24—Filed