FIELD: technological processes.
SUBSTANCE: invention can be used in production of welded structures and semi-finished products, including from aluminum alloys, by friction welding with mixing. One-sided thickening of parts being welded is performed by simultaneous cold deposition. Thickness and width of the thickening of the edges are selected to make the bearing capacity of the welded joint not less than that of the base metal. Width of bulge of each edge is not less than half of diameter of support collar of welding tool, and deepening of support collar into thickened edges of parts is performed by 0.1–0.2 mm.
EFFECT: possibility of welding without preliminary heating to produce a welded joint, which is not inferior in terms of bearing capacity to base metal.
3 cl, 5 dwg
Title | Year | Author | Number |
---|---|---|---|
APPARATUS FOR ARC BUTT WELDING OF PARTS | 0 |
|
SU859075A1 |
PRESSURE VESSEL, WELDING METHOD FOR ITS METAL SHELL, METHOD OF OBTAINING SPECIFIED CROSS-SECTION IN ROOT PART OF METAL SHELL WELD JOINT | 2007 |
|
RU2344337C1 |
TOOL FOR FRICTION STIR WELDING | 2015 |
|
RU2621514C2 |
METHOD OF FRICTION WELDING WITH MIXING OF ALUMINIUM ALLOYS | 2016 |
|
RU2634389C1 |
FRICTION WELDING METHOD WITH ALUMINIUM WROUGHT ALLOYS MIXING | 2016 |
|
RU2634402C1 |
METHOD OF COMBINED FRICTION WELDING OF TEE JOINTS | 2011 |
|
RU2466839C1 |
METHOD OF FRICTION WELDING BY MIXING | 2012 |
|
RU2509637C1 |
METHOD OF FRICTION WELDING WITH MIXING OF TEE JOINTS AND TOOL TO THIS END | 2009 |
|
RU2418664C1 |
LINE FOR MAKING PRECISE TUBES | 1994 |
|
RU2084300C1 |
METHOD OF ARE WELDING OF CIRCULAR JOINTS OF THIN-WALL SHELLS | 2008 |
|
RU2393946C2 |
Authors
Dates
2019-08-15—Published
2018-11-06—Filed