FIELD: chemistry.
SUBSTANCE: invention relates to fire-resistant moisture curable polymer compositions. Disclosed is a fire-resistant moisture-curable polymer composition comprising a polyolefin having hydrolysable silane groups, a halogenated polymer and a metal mercaptide. Invention also discloses cross-linked fire-resistant polymer composition obtained from said moisture-curable polymer composition, and conductor coated with cross-linked fire-resistant polymer composition.
EFFECT: disclosed composition has high fire-resistance and is easy to use.
8 cl, 24 tbl, 12 ex
Title | Year | Author | Number |
---|---|---|---|
STABILIZED MOISTURE-CURABLE POLYMER COMPOSITIONS | 2016 |
|
RU2733962C2 |
STABILIZED MOISTURE-CURABLE POLYMER COMPOSITIONS | 2016 |
|
RU2735228C2 |
MOISTURE-CURABLE COMPOSITION FOR INSULATION OF WIRE AND CABLE AND SHELL LAYERS | 2018 |
|
RU2769510C2 |
POLYOLEFIN-BASED SEMI-CRYSTALLINE SUPERCONCENTRATE COMPOSITION | 2017 |
|
RU2768478C2 |
SILANE-MODIFIED POLYMERS | 2009 |
|
RU2478655C2 |
ADDITIVE CONCENTRATE COMPOSITION BASED ON SEMICRYSTALLINE POLYOLEFIN | 2017 |
|
RU2766574C2 |
CROSS-LINKING ACCELERATORS FOR POLYMER COMPOSITIONS CONTAINING SILANE GROUPS | 2019 |
|
RU2779982C1 |
MOISTURE-CURED HOT-MELT ADHESIVES HAVING AT LEAST ONE SILANE GROUP-CONTAINING POLYURETHANE PREPOLYMER | 2006 |
|
RU2482136C2 |
MOIST-CURED POLYMER FOR FLEXIBLE CABLES | 2020 |
|
RU2784217C1 |
MODIFIED POLYOLEFINS | 2009 |
|
RU2496797C2 |
Authors
Dates
2019-08-21—Published
2015-05-20—Filed