FIELD: technological processes.
SUBSTANCE: invention can be used for welding with flux core of steel plates, including plates with high tensile strength and thick plates. In welding torch between contact tip and protective gas supply nozzle there installed is suction nozzle. Steel shell of wire with flux core has a seam produced by docking or overlapping of steel walls metal edges along length of wire. Wire has diameter of 1.2–2.0 mm and content of flux is 8–30 % of its total weight. Specifically, width of metal wire steel wire metal edges superimposition is limited.
EFFECT: method of welding using inexpensive seam wire with flux core ensures good weldability due to effective removal of hydrogen capable to diffusion when using suction nozzle and optimum design of welding wire.
8 cl, 4 dwg, 6 tbl
Title | Year | Author | Number |
---|---|---|---|
ELECTROGAS ARC WELDING METHOD AND ELECTROGAS ARC WELDING APPARATUS | 2015 |
|
RU2669668C2 |
LOW-ALLOYED STEEL OF WELDED SEAM AND WELD WIRE WITH FLUX CORE | 2006 |
|
RU2322529C2 |
WELDING WIRE FROM STAINLESS STEEL WITH FLUX CORE FOR WELDING STEEL SHEET AND METHOD OF ARC WELDING OF ZINC-COATED STEEL SHEET USING SAID WELDING WIRE | 2009 |
|
RU2482947C2 |
WELDING TORCH FOR FIRST ELECTRODE FOR MULTIPLATE SUBMERGED-ARC WELDING AND WELDING METHOD USING SUCH TORCH | 2013 |
|
RU2597186C2 |
WIRE WITH FLUX CORE | 2014 |
|
RU2638483C2 |
METHOD OF MULTI-ELECTRODE ARC WELDING IN PROTECTIVE GAS MEDIUM | 2018 |
|
RU2702168C1 |
WELDING DEVICE AND WELDING METHOD | 2016 |
|
RU2693248C2 |
METHOD FOR UNDERWATER WET WELDING AND CUTTING WITH CORE WIRE AND FLUX TAPE | 2021 |
|
RU2771341C1 |
WELDING TORCH | 2017 |
|
RU2697431C1 |
NANOSTRUCTURED FLUX CORD WIRE FOR UNDERWATER WELDING | 2013 |
|
RU2539284C1 |
Authors
Dates
2019-11-29—Published
2017-03-02—Filed