FIELD: chemistry.
SUBSTANCE: invention relates to glass melting and can be used for production of mineral wool. Crude mixture for feeding into a melting furnace, which provides for combustion of fuel, contains initial glass-lined material and biomass containing at least 50 wt.% of oil crops grains. and/or husks of grains of oil crops, such as sunflower, soya, rape, palm, peanut, olive, pumpkin. Mineral glass-lined material contains silicon oxide and at least an oxide or hydroxide or carbonate of an alkali and/or alkali-earth metal and is glass or rock or silicate.
EFFECT: reduced damage to equipment for dosing and transportation of initial glass-refined material, as well as partial replacement of fuel required for melting of glass-refined material.
15 cl, 1 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
FURNACE WITH IMMERSIBLE BURNER WITH SELF-LINING WALLS | 2018 |
|
RU2783785C2 |
BURNER INCLUDING A WEARABLE PART | 2018 |
|
RU2766104C2 |
MELTING APPARATUS OF SUBMERSIBLE COMBUSTION | 2016 |
|
RU2699114C2 |
BURNER FOR SUBMERSIBLE COMBUSTION MELTING UNIT | 2016 |
|
RU2715786C2 |
MINERAL FIBERS | 2018 |
|
RU2735595C1 |
FURNACE WITH SUBMERSIBLE BURNER | 2019 |
|
RU2776744C1 |
METHOD AND APPARATUS FOR POOL-FREE MELTING OF ROCK | 2002 |
|
RU2230709C2 |
METHOD FOR PREPARING OF BURDEN MATERIALS FOR GLASS MELTING AND APPARATUS FOR EFFECTUATING THE SAME (VERSIONS) | 2000 |
|
RU2266259C2 |
COMPOSITE CONTAINING MINERAL WOOL CONTAINING SUGAR | 2015 |
|
RU2690985C2 |
DEVICE AND METHOD OF FUSING VITRIFIABLE MATERIALS | 2002 |
|
RU2471727C2 |
Authors
Dates
2024-09-23—Published
2021-01-14—Filed