FIELD: residual fuel oil heat power stations ash processing. SUBSTANCE: during comminution of initial product iron-bearing reagent is added up to mass ratio of iron and nickel of 3.7 40 1 and than two staged burning with insertion of calcium-bearing addition is exercised. First stage is carried out with special consumption of air beginning from 6 m3/h per kg of charge. After burning hydrometallurgical treatment is exercised. Heat power electrical stations residual fuel oil slimes are used as iron-bearing reactant. EFFECT: increased share of nickel in concentrate and decrease of vanadium losses. 2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR EXTRACTING VANADIUM FROM THE ASHES OF THERMAL POWER PLANTS FROM THE COMBUSTION OF FUEL OIL | 2021 |
|
RU2775452C1 |
METHOD FOR PRODUCTION OF VANADIUM OXIDE ALLOY | 1986 |
|
SU1398445A1 |
METHOD OF COMPLEX REWORKING OF WASTES AFTER BURNING ORGANIC FUELS (VERSIONS) | 1998 |
|
RU2160318C2 |
METHOD OF OBTAINING VANADIUM PETROXIDE OF HIGH-PURITY | 1983 |
|
SU1208818A1 |
CHARGE FOR PRODUCING IRON ORE AGGLOMERATE | 2020 |
|
RU2752794C1 |
CHARGE FOR PRODUCTION OF IRON ORE AGGLOMERATE | 2023 |
|
RU2821213C1 |
MIX MATERIAL FOR PRODUCTION OF MANGANESE-CONTAINING STAFLUX | 2009 |
|
RU2410447C1 |
CHARGE FOR THE PRODUCTION OF IRON ORE AGGLOMERATE | 2021 |
|
RU2778807C1 |
PROCEDURE FOR METALLISATION OF TITANIUM-MAGNESIUM CONCENTRATES AT PRODUCTION OF IRON PELLETS AND TITANIUM-VANADIUM SLAG | 2008 |
|
RU2399680C2 |
METHOD OF PROCESSING VANADIUM CONTAINING IRON-TITANIUM CONCENTRATE | 2015 |
|
RU2606813C1 |
Authors
Dates
1995-11-20—Published
1986-01-14—Filed