FIELD: metallurgy. SUBSTANCE: heats of alloyed and low-carbon half-products are carried out in two aggregates. Low-carbon half-product is smelted from charge pig under temperature of 1580 - 1620 C. Then smelted half-products are mixed in ladle. EFFECT: increased steel impact toughness. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
ALLOYED STEELS PRODUCTION METHOD | 1985 |
|
SU1492715A1 |
PROCESS FOR PRODUCING ALLOY STEEL | 0 |
|
SU1752780A1 |
METHOD OF MAKING STEEL IN LIQUID STEEL MELTING BATH | 1990 |
|
RU2051180C1 |
BURDEN CHARGE AND STEEL SMELTING BURDEN | 1993 |
|
RU2042716C1 |
METHOD OF PRODUCTION OF HIGH-TEMPERATURE ALLOYS ON NICKEL BASE FOR SINGLE-CRYSTAL CASTING | 1987 |
|
SU1475172A1 |
METHOD OF SMELTING LOW-CARBON STEELS | 1996 |
|
RU2103379C1 |
METHOD FOR SMELTING RAIL STEEL | 0 |
|
SU1089149A1 |
METHOD OF PRODUCING ALLOY STEEL | 0 |
|
SU1382859A1 |
METHOD FOR PRODUCTION OF SYNTHETIC SLAG AND ALLOY FOR ALLOYING STEELS WITH NICKEL AND MOLYBDENUM | 1989 |
|
SU1678055A1 |
HIGH-GRADE ALLOY STEEL PRODUCING METHOD | 2005 |
|
RU2293125C1 |
Authors
Dates
1995-05-27—Published
1985-02-13—Filed