FIELD: refractory materials. SUBSTANCE: charge has, wt.-% periclase 40-85, and spinellide-containing component containing, vol. chrompicotite at refraction index N 2.00-2.09 85-90; periclase with inclusions of secondary spinellide at the ratio (93-96):(7-4) 7-11; silicates 1-6, and metallic phase 1-2. Properties of prepared refractory materials: onset point of softening under loading 0,2 H/mm2 is 1710-1720 C; thermal stability (1300 C, water) is 17-23 heat exchanges; wear of refractory materials is 1.5-2.0 mm/combustion x hr. EFFECT: increased wear resistance and thermal stability, decreased plastic deformation rate and toxicity. 1 dwg, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
MIXTURE FOR PRODUCTION OF COMPOSITIONS AND ARTICLES FOR STRUCTURALLY STABLE LININGS | 1997 |
|
RU2116275C1 |
PERICLASE-SPINEL REFRACTORY | 2015 |
|
RU2623760C2 |
COMPOSITION FOR PRODUCING PERICLASE-SPINELIDE REFRACTORIES | 2014 |
|
RU2570176C1 |
PERICLASE-SPINEL REFRACTORY PRODUCTS AND A METHOD FOR MANUFACTURE THEREOF | 2002 |
|
RU2235701C1 |
ROASTINGLESS REFRACTORY MATERIAL | 1982 |
|
RU2016875C1 |
CARBON-CONTAINING REFRACTORY PRODUCT | 1992 |
|
RU2040507C1 |
MAGNESIA-SPINELLIDE REFRACTORY MATERIAL | 2002 |
|
RU2198859C1 |
MASS FOR PRODUCTION OF BASIC REFRACTORY ARTICLES | 1995 |
|
RU2054394C1 |
MAGNESIA-SILICA REFRACTORY | 2001 |
|
RU2182140C1 |
MAGNESIA-SILICA REFRACTORY | 2000 |
|
RU2165396C1 |
Authors
Dates
1995-11-27—Published
1990-04-17—Filed