FIELD: cement industry. SUBSTANCE: mass composition, wt.-%: magnesite powder, 70-95; melted alumomanganese spinel, fraction 3-0 mm, activity degree 0.05-0.55 with content of < 0.1 mm fraction therein not over 25%, 5-30. EFFECT: increased compression strength, reduced open porosity and retarded high-temperature ageing of refractories during thermocycling. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
MASS FOR THE BASIC REFRACTORY ARTICLE MAKING | 1995 |
|
RU2085539C1 |
MIXTURE FOR PRODUCTION OF COMPOSITIONS AND ARTICLES FOR STRUCTURALLY STABLE LININGS | 1997 |
|
RU2116275C1 |
MASS FOR PERICLASE-SPINEL ARTICLE MAKING | 1995 |
|
RU2085538C1 |
PERICLASE-SPINEL REFRACTORY | 1998 |
|
RU2124487C1 |
MOLTEN SPINEL-CONTAINING MATERIAL | 1996 |
|
RU2076850C1 |
CARBON-CONTAINING REFRACTORY MATERIAL | 1996 |
|
RU2076849C1 |
MASS FOR MANUFACTURING REFRACTORY MATERIALS | 1997 |
|
RU2110583C1 |
SPINEL-PERICLASE-CARBON REFRACTORY MATERIAL | 1996 |
|
RU2068823C1 |
COMPOUND FOR MANUFACTURING PERICLASE-SPINLE REFRACTORIES | 1997 |
|
RU2148048C1 |
CHARGE TO MANUFACTURE PERICLASE-SPINEL PRODUCTS | 2010 |
|
RU2443657C1 |
Authors
Dates
1996-02-20—Published
1995-07-03—Filed