FIELD: polymeric materials. SUBSTANCE: copolymer has, mole%: vinyl acetate 43.4-51.6; butylacrylate 44.8-55; 1-methacryloyloxy-1-tert.-butylperoxyethane 0.8-5.1. Its intrinsic viscosity in acetone is 0.65-1.58 dl/g at 20 C. Copolymer is prepared by aqueous-emulsion polymerization of mixture monomers feeding in reaction zone at the constant rate 25-50% total loading per 1 h in the presence of 0.8-6 wt.-% emulsifying agent C-10 and water-soluble initiator which is loaded in equal time intervals - 24-48 min. EFFECT: improved method of making, enhanced quality of polymer. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ACRYL COPOLYMER FOR MANUFACTURE OF VIBRATION-ABSORBING MATERIAL AND PROCESS FOR EFFECTING SAME | 1990 |
|
SU1795644A1 |
ACRYL COPOLYMER FOR MANUFACTURE OF VIBRATION-ABSORBING MATERIAL AND PROCESS FOR EFFECTING SAME | 1990 |
|
SU1777337A1 |
COPOLYMER BASED ON VINYLACETATE AND BUTYLACRYLATE EMPLOYED AS POLYMERIC BASE FOR VIBRATION-ABSORBING MATERIAL AND PROCESS FOR MANUFACTURING SAME | 1990 |
|
SU1786811A1 |
VINYL ACETATE-BUTYL ACRYLATE COPOLYMER AS POLYMERIC SUBSTRATE OF VIBRATION ABSORBING MATERIAL AND PROCESS FOR PREPARING THEREOF | 1990 |
|
SU1757215A1 |
METHOD FOR PRODUCING VINYLACETATE-BUTYLACRYLATE COPOLYMER | 1988 |
|
SU1637284A1 |
METHOD OF PREPARING OF COPOLYMER OF VINYL ACETATE WITH BUTYLACRYLATE | 1988 |
|
SU1637285A1 |
METHOD FOR PRODUCING COPOLYMERS OF VINYL ACETATE WITH BUTYL ACRYLATE | 1988 |
|
SU1639007A1 |
METHOD FOR PRODUCING VINYLACETATE-BUTYLACRYLATE COPOLYMER | 1988 |
|
SU1653311A1 |
METHOD FOR PRODUCING COPOLYMERS OF VINYL ACETATE WITH BUTYL ACRYLATE | 1988 |
|
SU1639006A1 |
PROCESS FOR PRODUCING COPOLYMERS | 1990 |
|
SU1793702A1 |
Authors
Dates
1994-08-15—Published
1990-06-11—Filed