FIELD: chemistry. SUBSTANCE: acryl copolymer including 5.9 to 13.9 mole percent vinylacetate, 84.1 to 92.1 mole percent butylacrylate, 1.1 to 4.6 mole percent 1-methacryloyloxy-1-tert-butylperoxyethane exhibits inherent viscosity of 0.65 to 1.58 dl/g in acetone at temperature of 20 C. Desired product is produced by method of water-emulsion polymerization of monomer mixture introduced into reaction zone at constant rate of 33.3 to 50.0 % of total charge per 1 h in presence of 1 to 6 percent by mass emulsifier and water-soluble initiator charged by equal portions at equal intervals (24 to 36 min). EFFECT: excellent starting stock for manufacture of highly effective vibration-absorbing film materials. 2 tbl, 3 cl
Title | Year | Author | Number |
---|---|---|---|
ACRYL COPOLYMER FOR MANUFACTURE OF VIBRATION-ABSORBING MATERIAL AND PROCESS FOR EFFECTING SAME | 1990 |
|
SU1795644A1 |
COPOLYMER BASED ON VINYLACETATE AND BUTYLACRYLATE EMPLOYED AS POLYMERIC BASE FOR VIBRATION-ABSORBING MATERIAL AND PROCESS FOR MANUFACTURING SAME | 1990 |
|
SU1786811A1 |
ACRYLIC POLYMER FOR MAKING OF VIBRATING-ABSORBING MATERIAL AND A METHOD OF ITS MAKING | 1990 |
|
SU1771191A1 |
VINYL ACETATE-BUTYL ACRYLATE COPOLYMER AS POLYMERIC SUBSTRATE OF VIBRATION ABSORBING MATERIAL AND PROCESS FOR PREPARING THEREOF | 1990 |
|
SU1757215A1 |
METHOD FOR PRODUCING VINYLACETATE-BUTYLACRYLATE COPOLYMER | 1988 |
|
SU1637284A1 |
METHOD FOR PRODUCING COPOLYMERS OF VINYL ACETATE WITH BUTYL ACRYLATE | 1988 |
|
SU1639007A1 |
METHOD FOR PRODUCING COPOLYMERS OF VINYL ACETATE WITH BUTYL ACRYLATE | 1988 |
|
SU1639006A1 |
METHOD OF PREPARING OF COPOLYMER OF VINYL ACETATE WITH BUTYLACRYLATE | 1988 |
|
SU1637285A1 |
METHOD FOR PRODUCING VINYLACETATE-BUTYLACRYLATE COPOLYMER | 1988 |
|
SU1653311A1 |
AQUEOUS HETEROPOLYMERIC DISPERSION FOR PREPARING COVERS AND METHOD OF ITS PREPARING | 2000 |
|
RU2184125C1 |
Authors
Dates
1994-07-30—Published
1990-06-11—Filed