FIELD: chemistry. SUBSTANCE: acryl copolymer including 21.5 to 31.9 mole percent vinylacetate, 65.1 to 76.5 mole percent butylacrylate and 1.0 to 4.8 mole percent 1-methacryloyloxy-1-tert-butylperoxyethane has intrinsic viscosity of 0.54 to 1.22 dl/g in acetone at temperature of 20 C. Copolymer is produced by method of water-emulsion polymerization of monomer mixture admitted into reaction zone at constant rate of 28.5 to 50.0 % of total charge per 1 h in presence of 0.8 to 6.0 percent by mass emulsifier and water-soluble initiator charged by equal portions at equal intervals of 24 to 42 min. EFFECT: excellent stock for manufacture of vibration-absorbing materials. 3 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
COPOLYMER BASED ON VINYLACETATE AND BUTYLACRYLATE EMPLOYED AS POLYMERIC BASE FOR VIBRATION-ABSORBING MATERIAL AND PROCESS FOR MANUFACTURING SAME | 1990 |
|
SU1786811A1 |
ACRYL COPOLYMER FOR MANUFACTURE OF VIBRATION-ABSORBING MATERIAL AND PROCESS FOR EFFECTING SAME | 1990 |
|
SU1777337A1 |
VINYL ACETATE-BUTYL ACRYLATE COPOLYMER AS POLYMERIC SUBSTRATE OF VIBRATION ABSORBING MATERIAL AND PROCESS FOR PREPARING THEREOF | 1990 |
|
SU1757215A1 |
ACRYLIC POLYMER FOR MAKING OF VIBRATING-ABSORBING MATERIAL AND A METHOD OF ITS MAKING | 1990 |
|
SU1771191A1 |
METHOD OF PREPARING OF COPOLYMER OF VINYL ACETATE WITH BUTYLACRYLATE | 1988 |
|
SU1637285A1 |
METHOD FOR PRODUCING COPOLYMERS OF VINYL ACETATE WITH BUTYL ACRYLATE | 1988 |
|
SU1639007A1 |
METHOD FOR PRODUCING COPOLYMERS OF VINYL ACETATE WITH BUTYL ACRYLATE | 1988 |
|
SU1639006A1 |
METHOD FOR PRODUCING VINYLACETATE-BUTYLACRYLATE COPOLYMER | 1988 |
|
SU1653311A1 |
PROCESS FOR PREPARING TRIPLE COPOLYMERS | 1992 |
|
RU2049094C1 |
METHOD FOR PRODUCING VINYLACETATE-BUTYLACRYLATE COPOLYMER | 1988 |
|
SU1637284A1 |
Authors
Dates
1994-07-30—Published
1990-06-11—Filed