FIELD: building materials production. SUBSTANCE: 1 - 15 mm size grains of mixture of initial material and 70 - 90 % fuel are dried and enter crossflow shaft heater to be roasted for 6 - 20 min. in filtering bed at 1150 - 1350 C. Then the grains are unloaded and brought to electric kiln with 1450 C temperature. Dust carrying out decreased to 0.05 - 0.1 %, exhaust gas temperature is 100 C. EFFECT: higher efficiency. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF A TWO-STAGE CALCINATION OF THE GRANULAR AND GRAINED MATERIALS | 2001 |
|
RU2232362C2 |
METHOD FOR CEMENT CLINKER PRODUCTION | 1990 |
|
RU2031877C1 |
INSTALLATION FOR TWO-STAGE ROASTING OF GRANULATED AND GRANULAR MATERIALS | 2001 |
|
RU2214570C2 |
PROCESS FOR MANUFACTURE OF CEMENT CLINKER | 1989 |
|
RU2023698C1 |
SET FOR PRODUCING CEMENT CLINKER | 1990 |
|
RU2024805C1 |
METHOD FOR HIGH-SPEED MANUFACTURE OF ROASTING MOLDED PRODUCTS | 2001 |
|
RU2214574C2 |
SET FOR PRODUCING CEMENT CLINKER | 1990 |
|
RU2024809C1 |
METHOD FOR CEMENT PRODUCTION | 1990 |
|
SU1774608A1 |
INSTALLATION FOR HIGH-SPEED ROASTING OF MINERAL MATERIALS | 2001 |
|
RU2214571C2 |
METHOD FOR CEMENT CLINKER PRODUCTION | 1990 |
|
RU2032635C1 |
Authors
Dates
1996-06-20—Published
1986-05-27—Filed