FIELD: machine building. SUBSTANCE: solid particle of inoculator are added into stream of cast metal. Its quantity is determined according formula m = 100·М/P·[40C/L+C(Tl-20)], where m is quantity of solid particles of inoculator(kg), M is mass of cast melt (kg), P is desired porosity (%), C is specific heat capacity of melt, L is specific heat of fusion of particles, Tl is liquidus temperature (C), 40 is coefficient (C). Particles of said inoculator are identical to those of cast. EFFECT: improves distribution of porosity in thus prepared cast.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF CASTING HEAVY CASTINGS IN CASTING MOULD | 0 |
|
SU992117A1 |
METHOD OF PRODUCTION OF SHAPED CASTINGS | 2015 |
|
RU2638604C2 |
METHOD FOR PRODUCING INGOTS BY SQUEEZING COMBINED WITH CRYSTALLIZATION UNDER PRESSURE | 1990 |
|
RU2048253C1 |
METHOD OF CASTING OF METAL ALLOY CONTAINING PRIMARY PHASE DISPERSED IN EUTECTIC PHASE | 1994 |
|
RU2156176C2 |
METHOD TO PRODUCE EXTENDED THIN-WALLED CASTINGS | 1992 |
|
RU2034681C1 |
METHOD OF CENTRIFUGAL CAST OF MASSIVE BIMETALLIC ROLLERS WITH SOLID CROSS-SECTION | 2007 |
|
RU2338623C1 |
METHOD OF PRODUCING CASTINGS | 0 |
|
SU1306641A1 |
CLOSED ATMOSPHERIC CASTING HEAD | 1992 |
|
RU2074785C1 |
METHOD OF MODIFYING HEAT-RESISTANT ALLOYS AND HIGH-ALLOY STEELS | 2017 |
|
RU2701978C2 |
METHOD FOR PRODUCTION OF CONTINUOUSLY CAST HOLLOW BIMETALLIC BLANKS | 1995 |
|
RU2093299C1 |
Authors
Dates
1995-05-20—Published
1987-07-31—Filed