FIELD: production of welding equipment. SUBSTANCE: material contains 1.0-2.0% chromium, 0.5-0.7% zirconium, and copper the rest. Components are mixed, pressed, caked at 1020-1060 C for 4 h, left at 1060 C for 4 h, and hardened in water. EFFECT: increased stability and conductance of electrodes. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
DISPERSION-HARDENED MATERIAL FOR RESISTANCE WELLING ELECTRODES | 1996 |
|
RU2103135C1 |
PROCEDURE FOR TREATMENT OF SEMI-FINISHED PRODUCT OUT OF LOW ALLOYED DISPERSE-HARDENING COPPER ALLOY WITH CONTENTS OF NICKEL TO 1,6 %, BERRILIUM 0,2-0,8 % AND TITANIUM TO 0,15 % | 2009 |
|
RU2416672C1 |
DISPERSION-HARDNESS MATERIAL FOR ELECTRODES OF RESISTANCE WELDING | 1996 |
|
RU2104139C1 |
COPPER-BASE DISPERSION-HARDENED MATERIAL FOR WELDING | 1996 |
|
RU2103134C1 |
METHOD OF PREPARING OF POWDER ALLOY ON COPPER-BASE | 1990 |
|
RU2015851C1 |
MATERIAL FOR CURRENT-CONDUCTING TIPS | 0 |
|
SU1316773A1 |
DISPERSION-STRENGTHENED COMPOSITE MATERIAL FOR ELECTRIC CONTACT PARTS | 2001 |
|
RU2195511C2 |
METHOD OF PRODUCING ELECTRIC ARC PLASMA GENERATOR ELECTRODES | 2010 |
|
RU2455110C1 |
DISPERSEDLY HARDENED COMPOSITION MATERIAL | 1996 |
|
RU2113529C1 |
ELECTRODE FOR RESISTANCE SPOT WELDING | 2006 |
|
RU2337798C2 |
Authors
Dates
1996-11-27—Published
1989-12-04—Filed