FIELD: diamond production. SUBSTANCE: method involves mixing of explosive components trotyl and hexegen with addition of distilled water at concentration 12-15% of explosive substance mass. To improve physical stability of blasting charges the latters are pressed at 77± 2°C . EFFECT: toxic dust exhaust at mixing and loading of components in the mold is absent. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DETONATION SYNTHESIS OF NANODIAMONDS | 2017 |
|
RU2676614C1 |
METHOD AND PRIMARY PRODUCT FOR DETONATION SYNTHESIS OF POLYCRYSTALLINE DIAMOND | 2020 |
|
RU2748800C1 |
METHOD FOR INDUSTRIAL PRODUCTION OF DIAMONDS AND OTHER SOLID-PHASE NANOSTRUCTURED GRAPHITE FORMATIONS, APPARATUS AND CHARGE FOR PRODUCTION THEREOF | 2011 |
|
RU2483023C1 |
METHOD OF PREPARING NANO-DIAMANDS | 2003 |
|
RU2230702C1 |
NANODIAMOND AND METHOD OF ITS OBTAINMENT | 2005 |
|
RU2348580C1 |
METHOD FOR PRODUCTION OF DIAMONDS | 1993 |
|
RU2041166C1 |
METHOD FOR DETONATION SYNTHESIS OF POLYCRYSTALLINE DIAMOND | 2021 |
|
RU2774051C1 |
DIAMOND-CARBON SUBSTANCE AND METHOD OF ITS PRODUCTION | 1993 |
|
RU2041165C1 |
METHOD FOR DETONATION SYNTHESIS OF A POLYCRYSTALLINE DIAMOND | 2020 |
|
RU2757661C1 |
EXPLOSIVE SUBSTANCE FOR DETONATION SYNTHESIS OF DIAMOND AND A METHOD OF ITS PREPARING | 1995 |
|
RU2087455C1 |
Authors
Dates
1994-03-30—Published
1991-10-09—Filed