FIELD: investigation of physical-chemical and production processes. SUBSTANCE: operation of adhesiometer is based on breakage of specimen representing a coating in the form of a drop placed in the hole of a plate-cutter during whose movement on the surface of a fixed backing the hole generatrix breaks the sample due to the shearing force. The value of breaking load related to the contact area is the comparative characteristic of strength. At the same time the kind and nature of breakage are determined at investigation of formed surfaces. The method does not need production of standardized specimens, it is convenient at estimation of durability of the contact area. Adhesiometer dimensions - 80x100x300 mm, mass - 5 kg, time required to test a single specimen - 2 to 3 min. EFFECT: enhanced truth of determination of adhesion strength of materials. 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DETERMINING ADHESION STRENGTH OF COATING WITH BASE | 2013 |
|
RU2528575C1 |
METHOD OF EVALUATION OF ADHESIVE STRENGTH OF INSULATION COATING OF WINDINGS OF LOCOMOTIVE PROPELLING ENGINES AND DEVICE FOR ITS IMPLEMENTATION | 2017 |
|
RU2671548C1 |
PROCEDURE FOR EVALUATION OF ADHESION SHEAR STRENGTH OF HEAT SHIELDING COATING AND DEVICE FOR ITS IMPLEMENTATION | 2013 |
|
RU2548378C1 |
PROCESS OF DETERMINATION OF ADHESION OF GASOTHERMIC COAT | 1995 |
|
RU2084868C1 |
DEVICE FOR DETERMINING ADHESION STRENGTH OF MULTI-LAYER CERAMIC THERMAL-BARRIER COATING | 2016 |
|
RU2643682C1 |
METHOD OF MANUFACTURE OF SAMPLE FOR ADHESION STRENGTH TESTING | 1991 |
|
RU2067757C1 |
METHOD OF ASSESSING BONDING STRENGTH BETWEEN SCREEN-PRINTING INKS AND COATINGS WITH PRINT MEDIA | 2009 |
|
RU2390004C1 |
DEVICE THIN COATINGS SAMPLES FORMATION | 2018 |
|
RU2676953C1 |
METHOD FOR DETERMINING ADHESIVE STRENGTH OF GAS AND THERMAL BARRIER COATINGS | 1998 |
|
RU2146044C1 |
METHOD FOR EVALUATING THE ADHESIVE STRENGTH OF COATINGS AND APPARATUS FOR IMPLEMENTATION THEREOF | 2021 |
|