FIELD: metallurgy. SUBSTANCE: method for metal ladle treatment includes ladle addition of aluminum, silicon and manganese. Aluminum is added in the amount of 0.2-1.5 kg/t since the moment of starting the filling of ladle. Total amount of added manganese and silicon is determined by the formula given in the invention description. Manganese addition amounts to 1.1-2.4 of silicon addition. EFFECT: higher efficiency.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR CONTINUOUS CASTING OF RECTANGULAR BLANKS | 1993 |
|
RU2033887C1 |
BORON STEEL MAKING METHOD | 2011 |
|
RU2477324C1 |
METHOD OF PRODUCING BORON-CONTAINING STEEL | 2011 |
|
RU2492248C2 |
PROCEDURE FOR PRODUCTION OF HIGH CARBON ROD | 2008 |
|
RU2389802C2 |
METHOD OF PRODUCTION OF THE CARBON STEEL | 2006 |
|
RU2304622C1 |
METHOD FOR PRODUCING LOW-CARBON KILLED STEEL | 1997 |
|
RU2109074C1 |
METHOD OF STEEL DEOXIDATION | 0 |
|
SU572506A1 |
METHOD OF PROCESSING LOW-ALLOY STEEL IN THE PROCESS OF CONTINUOUS CASTING OF INGOTS | 1993 |
|
RU2037373C1 |
METHOD FOR PRODUCTION OF STEEL (VERSIONS) | 2014 |
|
RU2577885C1 |
METHOD OF RECEIVING OF HIGH-CARBON STEEL OF CORD QUALIT | 2008 |
|
RU2378391C1 |
Authors
Dates
1995-01-09—Published
1993-01-28—Filed