FIELD: manufacture of chemical power supply sources. SUBSTANCE: nickel hydroxide is mixed with graphite and solution of high-molecular binder in organic solvent. Substance diminishing dissolvability of binder is injected into obtained mixture, is mixed, applied to current tapping base and dried. After drying manufactured electrode is treated for 1-5 s in organic solvent where binder is dissolved and is dried at 20-100 C for the course of 1-10 h. EFFECT: enhanced capacitance and prolonged service life. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF FABRICATION OF NICKEL OXIDE ELECTRODE FOR NICKEL-ZINC BATTERY | 2014 |
|
RU2543057C1 |
PROCESS OF MANUFACTURE OF OXIDE-NICKEL ELECTRODE OF CHEMICAL POWER SUPPLY SOURCE | 1992 |
|
RU2016442C1 |
IRON ELECTRODE ACTIVE MASS OF NICKEL-IRON ACCUMULATOR | 2014 |
|
RU2586080C1 |
METHOD OF PRODUCING METAL-FELT BASES FOR OXIDE-NICKEL ELECTRODES OF ALKALINE ACCUMULATORS | 2015 |
|
RU2616584C1 |
METHOD OF MANUFACTURE OF DRY-CHARGED CADMIUM ELECTRODE | 1990 |
|
SU1809714A1 |
LITHIUM-CARBON ELECTROCHEMICAL CAPACITOR AND METHOD FOR PRODUCTION THEREOF | 2014 |
|
RU2581849C2 |
METHOD FOR PROCESSING LITHIUM-ION BATTERIES WITH OBTAINING POSITIVE ELECTRODE COMPONENTS OF ALKALINE BATTERIES | 2022 |
|
RU2789852C1 |
ACTIVE MASS OF NEGATIVE ELECTRODE OF NICKEL-HYDROGEN CELL | 1995 |
|
RU2084051C1 |
METHOD FOR PRODUCING NICKEL HYDROXIDE FOR ALKALI STORAGE BATTERIES | 2004 |
|
RU2264000C1 |
METHOD FOR MANUFACTURE OF ACTIVE MASS FOR ALKALINE BATTERY OXIDE-NICKEL FIBRE ELECTRODE | 2011 |
|
RU2475895C1 |
Authors
Dates
1995-02-27—Published
1992-09-30—Filed