FIELD: silicate industry. SUBSTANCE: protective coating has SiO2, Al2O3, TiO2, MgO, CaO and Fe2O3 taken at the following ratio, wt.-%: SiO2 2-6; Al2O3 61.5-65.0; TiO2 4.2-12.0; MgO 20.6-24.0; CaO 1.4-1.5, and Fe2O3 0.8-1.0. Use of proposed coating ensures to increase stability of lining to the effect of silicate melts at the boiling temperature below 1550 C. EFFECT: enhanced quality of coating. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
MOLTEN SPINEL-CONTAINING MATERIAL | 1996 |
|
RU2076850C1 |
CHARGE FOR MANUFACTURE OF ALUMINIUM-FERROUS SPINEL AND REFRACTORY USING ALUMINIUM-FERROUS SPINEL | 2013 |
|
RU2541997C1 |
METHOD OF APPLICATION OF COAT ON LINING OF ROTARY FURNACE | 1993 |
|
RU2075711C1 |
LINING OF ROTARY TUBULAR FURNACE FOR BURNING OF ORE-LIME MIXTURE | 1991 |
|
RU2037116C1 |
LUBRICANT FOR REFRACTORY METAL HOT PRESSING | 1999 |
|
RU2148615C1 |
MELT-MOULDED HIGH-CHROMIUM REFRACTORY MATERIAL | 2015 |
|
RU2581182C1 |
CARBON-CONTAINING REFRACTORY MATERIAL | 1997 |
|
RU2108311C1 |
MELTED FORSTERITE-CONTAINING MATERIAL AND REFRACTORY MATERIAL BASED THEREOF (VARIANTS) | 1999 |
|
RU2149856C1 |
PERICLASE-SPINEL REFRACTORY | 2015 |
|
RU2623760C2 |
MELT-MOULDED CHROMIUM-CONTAINING REFRACTORY MATERIAL | 2012 |
|
RU2495000C2 |
Authors
Dates
1995-03-27—Published
1992-10-08—Filed