FIELD: chemical technology. SUBSTANCE: oil coke is ground up to size less then 100 mcm, mixed with water taken at concentration 10-15% of coke mass, and subjected for thermal working at 850-950 C for 1-5 h at air feeding up to combustion loss 30-45%. EFFECT: improved method of producing. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF VANADIUM EXTRACTION FROM PETROLEUM COKE | 1992 |
|
RU2033449C1 |
SULFUR CONTAINING TITANIUM-VANADIUM MATERIAL PROCESSING METHOD | 1990 |
|
SU1782047A1 |
METHOD TO REPROCESS TITANIUM-MAGNETITE CONCENTRATES BEARING VANADIUM | 1991 |
|
RU2025524C1 |
METHOD OF PRODUCING POWDERED ACTIVATED CARBON | 2019 |
|
RU2722542C1 |
METHOD OF PRODUCING ACTIVATED CARBON | 2019 |
|
RU2724753C1 |
METHOD FOR DETERMINING ACTIVATION TIME OF OIL COKE SURFACE | 2011 |
|
RU2470983C1 |
METHOD OF DETERMINING OPTIMUM ACTIVATION TEMPERATURE OF CARBON MATERIALS | 0 |
|
SU747815A1 |
METHOD OF PURIFYING PETROLEUM- AND LUBE OIL-CONTAINING WASTE | 1998 |
|
RU2154617C2 |
METHOD OF PREPARING ACTIVATED ANTHRACITE | 2000 |
|
RU2177906C1 |
METHOD OF PRODUCING CARBONACEOUS ADSORBENT | 0 |
|
SU1789505A1 |
Authors
Dates
1995-05-10—Published
1992-05-28—Filed