FIELD: atomic power generation and chemical engineering industry. SUBSTANCE: method provides for hot deformation of blank, initial cold deformation and vacuum annealing under temperature of 560 590 C with isothermal holding for 3 4 hours, cold rolling and following final vacuum annealing under temperature of 560 585 C during 5 7 hours. EFFECT: method is used in atomic power generation and chemical engineering industry. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURE OF TUBULAR HEATING ELEMENT | 1990 |
|
RU2028575C1 |
METHOD FOR MANUFACTURE OF PRODUCTS FROM ZIRCONIUM AND ZIRCONIUM ALLOYS | 1992 |
|
RU2043890C1 |
METHOD FOR PRODUCING ARTICLES FROM ZIRCONIUM ALLOYS | 1996 |
|
RU2110600C1 |
METHOD OF PRODUCING PRODUCTS FROM THE ZIRCONIUM ALLOYS | 1993 |
|
RU2032760C1 |
PROCESS OF MANUFACTURE OF TUBULAR ARTICLES FROM ZIRCONIUM ALLOYS ( VERSIONS ) | 1997 |
|
RU2123065C1 |
METHOD FOR TREATMENT OF ZIRCONIUM | 1991 |
|
RU2021537C1 |
METHOD FOR MAKING ARTICLES OF ZIRCONIUM AND TITANIUM ALLOYS | 1997 |
|
RU2125916C1 |
METHOD FOR MANUFACTURING TUBULAR PRODUCTS FROM ZIRCONIUM-BASED ALLOY | 2019 |
|
RU2798022C1 |
METHOD FOR MANUFACTURING TUBULAR PRODUCTS FROM ZIRCONIUM ALLOY | 2019 |
|
RU2798020C1 |
METHOD FOR MANUFACTURING TUBULAR PRODUCTS FROM ZIRCONIUM ALLOY | 2019 |
|
RU2798021C1 |
Authors
Dates
1995-06-19—Published
1992-12-21—Filed