FIELD: production of enamel. SUBSTANCE: proposed enamel slip contains (mass parts): frit 100, clay 4-7, borax 0.05-0.5, finely ground sand 0.1-10, electrolyte 0.05-0.2, pigments 2-5, water 35-45. Aforementioned frit contains (mass %): silicium oxide having essential formula SiO2, 42-48, boron oxide having essential formula B2O3 13-15, potassium oxide having essential formula K2O 3-5, sodium oxide having essential formula Na2O 18-21, zirconium oxide having essential formula ZrO2 2-5, zinc oxide having essential formula ZnO 2-5, calcium oxide having essential formula CaF2 5-7, aluminium oxide having essential formula Al2O3, 3-5, lithium oxide having essential formula Li2O. 1-3. EFFECT: improves quality of desired product. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
ENAMEL | 1993 |
|
RU2041174C1 |
METHOD OF PREPARING ENAMEL COATING | 1998 |
|
RU2154036C2 |
SILICATE ENAMEL COATING FOR INTERNAL PROTECTION OF STEEL PIPELINES | 2020 |
|
RU2769688C2 |
PRIMER ENAMEL FRIT FOR APPLYING BY ELECTROSTATIC METHOD | 1994 |
|
RU2127710C1 |
ENAMEL | 2006 |
|
RU2332369C1 |
COMPOSITION OF GLASS-CRYSTAL COATING FOR STEEL CHEMICAL EQUIPMENT | 2018 |
|
RU2750530C2 |
ENAMEL | 1995 |
|
RU2098368C1 |
PROTECTIVE COMPOSITE GLASS-ENAMEL COATING FOR STEEL AND METHOD OF PREPARATION THEREOF | 1998 |
|
RU2145583C1 |
ENAMEL SLIP | 0 |
|
SU1555307A1 |
ENAMEL SLIP FOR PRIMER-FREE COATING | 1996 |
|
RU2116271C1 |
Authors
Dates
1996-08-20—Published
1993-07-30—Filed