FIELD: production of thin-sheet electrical steel. SUBSTANCE: normalization of hot-rolled steel of sulfonitride melting version is carried out with regulated cooling whose rate vc down to 750-900 C is established depending on the content of aluminium in steel. Decarburizing annealing is effected with regulated heating rate vh depending on vc. Steel treated in compliance with the offered method features extremely high values of magnetic induction B100 and low level of specific losses P1,7 without intermelt discontinuity. EFFECT: higher efficiency. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ELECTROTECHNICAL ANISOTROPIC STEEL PRODUCTION METHOD | 1992 |
|
RU2048543C1 |
METHOD FOR HEAT-TREATMENT OF ANISOTROPIC ELECTRIC STEEL | 1990 |
|
RU2022034C1 |
METHOD FOR MAKING ANISOTROPIC ELECTRICAL STEEL | 2002 |
|
RU2199594C1 |
PROCESS FOR MAKING COLD ROLLED ELECTRICAL ANISOTROPIC STEEL | 2002 |
|
RU2199595C1 |
METHOD FOR PRODUCING ELECTRICAL STEEL WITH HIGH MAGNETIC DENSITY | 2002 |
|
RU2216601C1 |
PROCEDURE FOR PRODUCTION OF ANISOTROPIC ELECTRO-TECHNICAL STEEL WITH HIGH MAGNETIC PROPERTIES | 2009 |
|
RU2407809C1 |
METHOD FOR PRODUCING ANISOTROPIC ELECTRICAL STEEL | 1994 |
|
RU2082772C1 |
METHOD OF MAKING ELECTRICAL-SHEET ANISOTROPIC STEEL | 2001 |
|
RU2175985C1 |
METHOD FOR MAKING ANISOTROPIC ELECTRICAL STEEL | 0 |
|
SU1813105A3 |
SILICON ELECTRIC STEEL AND METHOD OF TREATMENT THEREOF | 1996 |
|
RU2096516C1 |
Authors
Dates
1996-10-27—Published
1990-09-10—Filed