FIELD: ferrous metallurgy; making grain-oriented electrical- sheet steels at high permeability of magnetic flux. SUBSTANCE: method consists in maximum realization of principle of grain- oriented heredity in production line making electrical-sheet anisotropic steel. Method includes heating of steel before hot rolling in temperature range ensuring single-phase (ferrite) structure; time and temperature conditions of hot deformation of metal at which 3 to 8% of austenite appears in temperature range from 1100 to 1150 C; method includes also heating of steel for primary recrystallization after second cold rolling procedure at rather slow rate. EFFECT: high magnetic properties of steel made according to this method. 3 cl, 1 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF ANTISOTROPIC ELECTRICAL STEEL | 1999 |
|
RU2142020C1 |
PROCESS FOR MAKING COLD ROLLED ELECTRICAL ANISOTROPIC STEEL | 2002 |
|
RU2199595C1 |
METHOD FOR PRODUCING ELECTRICAL STEEL WITH HIGH MAGNETIC DENSITY | 2002 |
|
RU2216601C1 |
METHOD TO PRODUCE HIGHLY PERMEABLE ANISOTROPIC ELECTRIC STEEL | 2012 |
|
RU2516323C1 |
METHOD OF PRODUCTION OF ANISOTROPIC ELECTRICAL STEEL | 1999 |
|
RU2142019C1 |
METHOD FOR MAKING COLD ROLLED ELECTRICAL ANISOTROPIC STEEL | 2001 |
|
RU2180356C1 |
PROCESS OF PRODUCTION OF GRAIN-ORIENTED ELECTRICAL-SHEET STEEL WITH LIMITED ANISOTROPY, STRIP PRODUCED BY THIS PROCESS AND ARTICLE FROM IT | 2001 |
|
RU2180924C1 |
METHOD OF ELECTROTECHNICAL ANISOTROPIC STEEL MANUFACTURING WITH INCREASED CONDUCTIVITY | 2006 |
|
RU2348705C2 |
METHOD FOR MAKING ELECTRICAL ANIZOTROPIC STEEL | 2001 |
|
RU2182181C1 |
METHOD FOR MAKING COLD ROLLED STRIP OF ELECTRICAL ANISOTROPIC STEEL | 2001 |
|
RU2180357C1 |
Authors
Dates
2001-11-20—Published
2001-04-19—Filed