FIELD: ferrous metallurgy. SUBSTANCE: method for making cold rolled strip of electrical steels with texture (110)[001], namely making steel with AlN-phase as inhibitor of standard growing of grains after hot rolling of strip or only after cold rolling comprises steps of additional treatment for enlarging grain structure; after hot rolling or only after cold rolling with small deformation degree subjecting strip to additional annealing in hood furnace at 750- 900 C. EFFECT: high stable magnetic properties of electrical anisotropic steel due to optimal combination of technological processes important for formation of texture and inhibitor phase. 4 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MAKING COLD ROLLED STRIP OF ELECTRICAL ANISOTROPIC STEEL | 2001 |
|
RU2180357C1 |
PROCESS OF PRODUCTION OF GRAIN-ORIENTED ELECTRICAL-SHEET STEEL WITH LIMITED ANISOTROPY, STRIP PRODUCED BY THIS PROCESS AND ARTICLE FROM IT | 2001 |
|
RU2180924C1 |
METHOD OF PRODUCTION OF ANISOTROPIC ELECTRICAL- SHEET STEEL | 2000 |
|
RU2159821C1 |
METHOD FOR MAKING ELECTRICAL ANIZOTROPIC STEEL | 2001 |
|
RU2182181C1 |
METHOD OF MAKING ELECTRICAL-SHEET ANISOTROPIC STEEL | 2001 |
|
RU2175985C1 |
METHOD OF PRODUCTION OF ANTISOTROPIC ELECTRICAL STEEL | 1999 |
|
RU2142020C1 |
ANISOTROPIC ELECTRICAL STEEL AND METHOD OF ITS PRODUCTION | 2001 |
|
RU2181786C1 |
METHOD OF ELECTROTECHNICAL ANISOTROPIC STEEL MANUFACTURING WITH INCREASED CONDUCTIVITY | 2006 |
|
RU2348705C2 |
PROCESS FOR MAKING COLD ROLLED ELECTRICAL ANISOTROPIC STEEL | 2002 |
|
RU2199595C1 |
METHOD OF ELECTROTECHNICAL ANISOTROPIC STEEL PRODUCTION WITH INCREASED CONDUCTIVITY | 2006 |
|
RU2348704C2 |
Authors
Dates
2002-03-10—Published
2001-07-06—Filed