FIELD: ferrous metallurgy. SUBSTANCE: method includes hot rolling of steel containing (in wt %): silicon, 2.8-3.2; manganese, 0.1-0.3; copper, 0.1-0.7; and aluminium, 0.010-0.30 at coiling temperature 530-650 C, double cold rolling, intermediate decarbonizing baking, and final high-temperature annealing. Improvement of electromagnetic properties of anisotropic electrical steel and reduction of its production cost price is achieved by reducing, in the course of hot rolling, coiling temperature as weight part of aluminium in steel rises. When this part is 0.010-0.014%, coiling temperature is 650-580 C, and with 0.015-0.030% aluminium, 579-530 C. EFFECT: improved electromagnetic properties of product. 3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING ANISOTROPIC ELECTRICAL STEEL | 1994 |
|
RU2082771C1 |
SILICON ELECTRIC STEEL AND METHOD OF TREATMENT THEREOF | 1996 |
|
RU2096516C1 |
MANUFACTURING METHOD OF ANISOTROPIC ELECTROTECHNICAL STEEL | 2009 |
|
RU2403293C1 |
METHOD OF PRODUCING ANISOTROPIC ELECTRICAL-SHEET STEEL | 1999 |
|
RU2150518C1 |
METHOD OF PRODUCTION OF SHEET ELECTROTECHNICAL ANISOTROPIC STEEL | 2003 |
|
RU2233892C1 |
PROCESS OF PRODUCTION OF ANISOTROPIC ELECTRICAL SHEET STEEL | 1996 |
|
RU2098493C1 |
PROCEDURE FOR PRODUCTION OF ANISOTROPIC ELECTRO-TECHNICAL STEEL WITH HIGH MAGNETIC PROPERTIES | 2009 |
|
RU2407809C1 |
METHOD OF BLACK PLATE PRODUCTION | 1999 |
|
RU2165465C1 |
ANISOTROPIC ELECTRICAL STEEL PRODUCTION PROCESS | 1997 |
|
RU2118382C1 |
METHOD OF PRODUCTION OF COLD ROLLER ELECTRICAL-SHEET ISOTROPIC STEEL | 1999 |
|
RU2155233C1 |
Authors
Dates
1997-06-27—Published
1994-09-20—Filed