FIELD: manufacture of chemical power supplies. SUBSTANCE: 100 mass parts of active material are mixed up with 2.4-24 mass parts of binder (water dispersion of butadient and organic substance copolymer) and 10-40 mass parts of water; mixture obtained is applied to current lead and dried out. EFFECT: improved mechanical strength of electrode, facilitated manufacture. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURING OF LITHIUM-ION ACCUMULATOR ELECTRODES | 2008 |
|
RU2390078C1 |
METHOD FOR MANUFACTURING OF LITHIUM-ION ACCUMULATOR ELECTRODES | 2014 |
|
RU2547819C1 |
LITHIUM-POLYMER BATTERY AND METHOD OF ITS MANUFACTURING | 2014 |
|
RU2564201C1 |
POLYMER ELECTROLYTE GEL FOR LITHIUM-ION BATTERY | 2011 |
|
RU2457587C1 |
STORAGE BATTERY | 1993 |
|
RU2107360C1 |
NITRILE BUTADIENE LATEX, DIP LATEX COMPOSITION, DIP PRODUCT | 2021 |
|
RU2771752C1 |
ELECTRODE FOR ALKALI STORAGE BATTERY AND METHOD FOR ITS MANUFACTURING | 1995 |
|
RU2098891C1 |
BUTADIENE-NITRILE LATEX, LATEX COMPOSITION FOR IMMERSION DIPPING, DIPPED PRODUCT | 2021 |
|
RU2776174C1 |
METHOD OF OBTAINING LATEX | 2017 |
|
RU2676609C1 |
METHOD FOR MANUFACTURING OF LITHIUM-ION ACCUMULATOR ELECTRODES | 2009 |
|
RU2383086C1 |
Authors
Dates
1997-01-10—Published
1994-11-29—Filed